Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ultimate Bearing Strength | 349 MPa | 50600 psi | Average value longitudinal with bearing strain 8.9%. |
Materion AlBeMet® AM 162 Extruded Bar, Annealed Mechanical property values below are in the longitudinal direction; transverse values generally lower. This is a powder metallurgical product produced by gas atomization available as rod, bar, tube.. |