Mechanical Properties Metric English Comments
Ultimate Bearing Strength 333 MPa
48300 psi
Average value longitudinal-transverse is 333 MPa w/ bearing strain 6.4%. e/D = 1.5.
Materion AlBeMet® AM 162 Extruded Bar, Annealed
Mechanical property values below are in the longitudinal direction; transverse values generally lower. This is a powder metallurgical product produced by gas atomization available as rod, bar, tube..