Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ultimate Bearing Strength | 333 MPa | 48300 psi | Average value longitudinal-transverse is 333 MPa w/ bearing strain 6.4%. e/D = 1.5. |
Materion AlBeMet® AM 162 Extruded Bar, Annealed Mechanical property values below are in the longitudinal direction; transverse values generally lower. This is a powder metallurgical product produced by gas atomization available as rod, bar, tube.. |