Mechanical Properties Metric English Comments
Puncture Energy 10.5 J
7.74 ft-lb
ASTM D3763
Chevron Phillips MarFlex® D163 Metallocene Linear Low Density Polyethylene, Blown Film
This mLLDPE is tailored for applications that require:Excellent clarityExcellent glossExcellent toughnessExcellent heat sealTypical blown film applications include:Seal layer in coextrusionsHeavy du..