Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips MarFlex® D163 Metallocene Linear Low Density Polyethylene, Blown Film

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer Chevron Phillips Chemical Company LP
Trade Name MarFlex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips MarFlex® D163 Metallocene Linear Low Density Polyethylene, Blown Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This mLLDPE is tailored for applications that require:Excellent clarityExcellent glossExcellent toughnessExcellent heat sealTypical blown film applications include:Seal layer in coextrusionsHeavy duty packagingClarity packagingThis grade contains a process aid and does not contain antiblock or slip agent.Information provided by Chevron Phillips Chemical Company LP.
Physical Properties Metric English Comments
Density 0.914 g/cc
0.0330 lb/in³
ASTM D1505
Melt Flow 0.90 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.90 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 10.0 MPa
1450 psi
ASTM D882
Film Tensile Strength at Yield, TD 9.00 MPa
1310 psi
ASTM D882
Film Elongation at Break, MD 500 %
500 %
ASTM D882
Film Elongation at Break, TD 600 %
600 %
ASTM D882
Puncture Energy 10.5 J
7.74 ft-lb
ASTM D3763
Coefficient of Friction >= 1.0
>= 1.0
ASTM D1894
Elmendorf Tear Strength, MD 10.6 g/micron
270 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 14.2 g/micron
360 g/mil
ASTM D1922
Dart Drop 59.1 g/micron
1500 g/mil
ASTM D1709
Film Tensile Strength at Break, MD 61.0 MPa
8850 psi
ASTM D882
Film Tensile Strength at Break, TD 50.0 MPa
7250 psi
ASTM D882
1% Secant Modulus, MD 146 MPa
21200 psi
ASTM D882
1% Secant Modulus, TD 165 MPa
23900 psi
ASTM D882
Heat Seal Strength Initiation Temperature 95.0 °C
203 °F
ASTM F882
Optical Properties Metric English Comments
Haze 4.0 %
4.0 %
ASTM D1003
Gloss 135 %
135 %
at 60°; ASTM D2457
Descriptive Properties Value Comments
Film Puncture Force 129 N
ASTM D3763
Process Film
Region Mexico
Bamberger Polymers Distribution
Copyright © lookpolymers.com All Rights Reserved