Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 64.0 - 64.0 J @Temperature -30.0 - -30.0 °C |
47.2 - 47.2 ft-lb @Temperature -22.0 - -22.0 °F |
Average value: 64.0 J Grade Count:1 |
Overview of materials for Nylon 6, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro.. |
|||
Puncture Energy | 64.0 - 64.0 J @Temperature -30.0 - -30.0 °C |
47.2 - 47.2 ft-lb @Temperature -22.0 - -22.0 °F |
Average value: 60.9 J Grade Count:1 |
Overview of materials for Nylon 6, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri.. |