Mechanical Properties Metric English Comments
Puncture Energy 64.0 - 64.0 J

@Temperature -30.0 - -30.0 °C
47.2 - 47.2 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 64.0 J Grade Count:1
Overview of materials for Nylon 6, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro..
Puncture Energy 64.0 - 64.0 J

@Temperature -30.0 - -30.0 °C
47.2 - 47.2 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 60.9 J Grade Count:1
Overview of materials for Nylon 6, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri..