Polymer Property : Puncture Energy = 6.91 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 6.91 J
5.10 ft-lb
Dow Method
Dow ELITE™ 5110G Enhanced Polyethylene Resin
™ 5110G is a copolymer produced via INSITE™ Technology from Dow Plastics. It offers a unique combination of high modulus and excellent impact strength, allowing for down gauging in bag applicatio..