Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Puncture Energy = 6.21 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 6.21 J
4.58 ft-lb
ExxonMobil Method
ExxonMobil EXACT™ 4053 Cast Plastomer
Product Description: Exact 4053 is an ethylene-based butene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. This resin is designed primarily for use in blends with poly..
Copyright © lookpolymers.com All Rights Reserved