Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 6.21 J | 4.58 ft-lb | ExxonMobil Method |
ExxonMobil EXACT™ 4053 Cast Plastomer Product Description: Exact 4053 is an ethylene-based butene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. This resin is designed primarily for use in blends with poly.. |