Polymer Property : Puncture Energy = 4.00 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 5.42 J
4.00 ft-lb
ExxonMobil Method
ExxonMobil Exact™ 3040 Cast Ethylene-based Plastomer Resin
Product Description: Exact 3040 is an ethylene-based hexane copolymer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 3040 is designed for monolayer and coextrusion cast fi..
Puncture Energy 5.42 J
4.00 ft-lb
Dow Method
Dow TUFLIN™ HS-7066 NT 7 Linear Low Density Polyethylene Resin
Hexene Linear Low Density Resin Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a TUFLIN™ HS-7066 NT 7 is a fractional melt, ethylene-hexene copolymer, designed for good toughness and stiffness. Th..