Polymer Property : Puncture Energy = 32.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 2.00 - 32.0 J

@Temperature -30.0 - -30.0 °C
1.48 - 23.6 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 15.5 J Grade Count:6
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim..
Puncture Energy 2.00 - 32.0 J

@Temperature -30.0 - -30.0 °C
1.48 - 23.6 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 17.6 J Grade Count:5
Overview of materials for Polybutylene Terephthalate (PBT), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Extrusion Grade". Each property range of values reported is minimum an..
Puncture Energy 3.80 - 32.0 J
2.80 - 23.6 ft-lb
Average value: 11.4 J Grade Count:4
Overview of materials for Nylon 6, Glass Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu..