Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Puncture Energy = 2.80 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 3.80 - 32.0 J
2.80 - 23.6 ft-lb
Average value: 11.4 J Grade Count:4
Overview of materials for Nylon 6, Glass Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu..