Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 3.13 J | 2.31 ft-lb | ExxonMobil |
ExxonMobil LL 1001x72 Blown Film Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Puncture Energy | 3.13 J | 2.31 ft-lb | ExxonMobil |
ExxonMobil LL 1001x74 Blown Film Resin LL1001 are butene LLDPE blown film resins having good drawdown, tensile and toughness properties.Information provided by ExxonMobil Chemical |
|||
Puncture Energy | 3.13 J | 2.31 ft-lb | ExxonMobil |
ExxonMobil LL 1001x76 Blown Film Resin LL1001 are butene LLDPE blown film resins having good drawdown, tensile and toughness properties.Information provided by ExxonMobil Chemical |
|||
Puncture Energy | 3.13 J | 2.31 ft-lb | ExxonMobil |
ExxonMobil LL 1001x59 Blown Film Resin
(discontinued **) LL1001 are butene LLDPE blown film resins having good drawdown, tensile and toughness properties.Information provided by ExxonMobil Chemical |