Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 10.0 - 30.0 J @Temperature -30.0 - -30.0 °C |
7.38 - 22.1 ft-lb @Temperature -22.0 - -22.0 °F |
Average value: 19.0 J Grade Count:5 |
Overview of materials for Polycarbonate, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea.. |