Mechanical Properties Metric English Comments
Puncture Energy 3.70 J
2.73 ft-lb
Conditioned; ISO 6603-2
Lanxess Durethan® AKV 30 GIT H2.0 900116 Nylon 66, 30% Glass Fiber
PA 66, injection molding grade, 30% glass fibers, suitable for GIT (gas assisted technology), good surface finish, good heat-ageing resistance
Puncture Energy 3.70 J

@Temperature -30.0 °C
2.73 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Durethan® BKV 50 H2.0 901510 Nylon 6, 50% Glass Fiber
PA 6, injection molding grade, 50% glass fibers, good heat-ageing resistance
Puncture Energy 3.70 J

@Temperature -30.0 °C
2.73 ft-lb

@Temperature -22.0 °F
Conditioned; ISO 6603-2
Lanxess Durethan® BKV 50 H2.0 901510 Nylon 6, 50% Glass Fiber
PA 6, injection molding grade, 50% glass fibers, good heat-ageing resistance