Mechanical Properties Metric English Comments
Puncture Energy 0.800 - 24.0 J

@Temperature -40.0 - -40.0 °C
0.590 - 17.7 ft-lb

@Temperature -40.0 - -40.0 °F
Average value: 7.77 J Grade Count:4
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m..
Puncture Energy 0.800 - 24.0 J

@Thickness 2.50 - 3.20 mm
0.590 - 17.7 ft-lb

@Thickness 0.0984 - 0.126 in
Average value: 7.77 J Grade Count:4
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m..