Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 1.80 - 10.6 J | 1.33 - 7.82 ft-lb | Average value: 4.07 J Grade Count:4 |
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15.. |