Mechanical Properties Metric English Comments
Puncture Energy 2.03 J
1.50 ft-lb
ExxonMobil Method
ExxonMobil LD 123.LN General Purpose Clarity Film Resin
Product Description: LD 123.LN blown film grade offers an excellent balance of optical and strength properties for general purpose clear film applications.Availability: Latin America, North America ..
Puncture Energy 2.03 J
1.50 ft-lb
ExxonMobil Method
ExxonMobil LDPE LD 123.LN Low Density Polyethylene Resin
Product Description: LD 123.LN blown film grade offers an excellent balance of optical and strength properties for general purpose clear film applications.Availability: Latin America, North America ..