Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 0.757 J | 0.558 ft-lb | ExxonMobil Method |
ExxonMobil LD 105.30 Very High Clarity Packaging Film Resin Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or.. |
|||
Puncture Energy | 0.757 J | 0.558 ft-lb | ExxonMobil Method |
ExxonMobil LD 105.BR Very High Clarity Packaging Film Resin Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or.. |
|||
Puncture Energy | 0.757 J | 0.558 ft-lb | ExxonMobil Method |
ExxonMobil LDPE LD 105.30 Low Density Polyethylene Resin Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or.. |
|||
Puncture Energy | 0.757 J | 0.558 ft-lb | ExxonMobil Method |
ExxonMobil LDPE LD 105.BR Low Density Polyethylene Resin Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or.. |