Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 0.700 J @Temperature -30.0 °C |
0.516 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Durethan® AKV 15 H2.0 901510 Nylon 66, 15% Glass Fiber PA 66, injection molding grade, 15% glass fibers, good heat-ageing resistance |
|||
Puncture Energy | 0.700 J @Temperature -30.0 °C |
0.516 ft-lb @Temperature -22.0 °F |
Conditioned; ISO 6603-2 |
Lanxess Durethan® AKV 15 H2.0 901510 Nylon 66, 15% Glass Fiber PA 66, injection molding grade, 15% glass fibers, good heat-ageing resistance |