Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 0.500 J | 0.369 ft-lb | ASTM D5748 |
Borealis Himod™ FT6273 LDPE for Film Himod FT6273 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i.. |
|||
Puncture Energy | 0.500 J | 0.369 ft-lb | ASTM D5748 |
Borealis Himod™ FT6274 LDPE for Film Himod FT6274 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i.. |