Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Unnotched | 130 J @Treatment Temp. 177 °C |
95.9 ft-lb @Treatment Temp. 350 °F |
tempered at 350°F |
Carpenter Vega® Alloy Tool Steel (Air-Tough) (AISI A6) Vega die steel combines the deep hardening and minimum size change characteristics of air-hardening steels with the simplicity of low temperature heat treatment possible in many oil-hardening steels.. |