Flexural Modulus 6.63 GPa
962 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-KON RFD03 PA 66
LNP* STAT-KON* RFD03 is a compound based on Nylon 66 containing 15% Glass Fiber. Added feature of this material is: Electrically Conductive.
Flexural Modulus 6.63 GPa
962 ksi
ISO Data
BASF Nypel® 2367G HS BK 15/25% Glass/Mineral Filled PA6 (Dry)
Nypel 2367G HS BK-4 is a black pigmented, heat stabilized, 40% mineral and glass fiber reinforced injection molding compound based on recycled PA6 feedstocks. It possesses a balance of engineering ..