Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.662 GPa | 96.0 ksi | ASTM D790 |
ExxonMobil Escorene® HD-6706 HDPE, Injection Grade
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Excellent Impact, Good Stiffness, Excellent ESCRUses: Pails, Industrial containers, Structural foams |