Mechanical Properties Metric English Comments
Flexural Modulus 0.662 GPa
96.0 ksi
ASTM D790
ExxonMobil Escorene® HD-6706 HDPE, Injection Grade  (discontinued **)
Data Provided by Exxon Chemical Canada.Characteristics: Excellent Impact, Good Stiffness, Excellent ESCRUses: Pails, Industrial containers, Structural foams