POLYMER SEARCH
Polymer Property : Flexural Modulus = 9.501 GPa
Polymer Property :
Flexural Modulus =
9.501 GPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Flexural Modulus
9.501
GPa
1378
ksi
ASTM D790
PlastxWorld Veroplas PB3500 Nylon 66
general purpose, 50% glass filled injection molding gradeInformation provided by PlastxWorld Inc.