Mechanical Properties Metric English Comments
Flexural Modulus 60.0 GPa
8700 ksi
Material as cured; RT
Hexcel® HexPly® 922-1/35%/G926 180°C Curing Epoxy Matrix
5H satin/370g/m2 carbon fabric: FVC=60%Information provided by HexCel
Flexural Modulus 60.0 GPa
8700 ksi
Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix, High Strength 6k carbon Balanced fabric 285 g/m2
Information provided by HexCel