Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.597 GPa | 86.6 ksi | ASTM D790 |
PlastxWorld CEVIAN® A5624 20% GF PA/ABS Alloy, DAM Property data is for dry as molded (DAM) samples.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Flexural Modulus | 0.597 - 8.13 GPa | 86.6 - 1180 ksi | Average value: 4.49 GPa Grade Count:20 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo.. |