Flexural Modulus 0.597 GPa
86.6 ksi
ASTM D790
PlastxWorld CEVIAN® A5624 20% GF PA/ABS Alloy, DAM
Property data is for dry as molded (DAM) samples.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Flexural Modulus 0.597 - 8.13 GPa
86.6 - 1180 ksi
Average value: 4.49 GPa Grade Count:20
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo..