Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 5.92 GPa
859 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON DX02728C PC
LNP STAT-KON* DX02728C is a compound based on Polycarbonate resin containing Proprietary Filler(s) Added features of this material include: Clean Compounding System, Electrically Conductive.
Flexural Modulus 5.92 GPa
859 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Thermocomp OB008 PPS - Branched
LNP* Thermocomp* OB008 is a compound based on Branched PPS containing Glass Beads.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 5.92 GPa
859 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP QF004 PA 6/10
LNP* THERMOCOMP* QF004 is a compound based on Nylon 6/10 resin containing 20% Glass Fiber.
Flexural Modulus 5.92 GPa
859 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP QF004 PA 6/10 (Asia Pacific)
LNP* Thermocomp* QF004 is a compound based on Nylon 6/10 resin containing Glass Fiber.
Flexural Modulus 5.92 GPa
859 ksi
ISO 178
Ecomass® 3011ZD86 Tungsten Filled Polycarbonate
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsHigh Specific GravityTungsten Filled Polycarbonate (PC) CompoundGood ToughnessInformation provided by Tech..