Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.77 GPa | 837 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL ZM3242 PPE+PS (Asia Pacific) Modified PPO* 30% mineral filled products, Non Halogenated Flame Retardant V-1 products.Supper low warpage series, HDT 110degC |
|||
Flexural Modulus | 5.77 GPa | 837 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp ZM3242 PPE+PS (Asia Pacific) Modified PPO* 30% mineral filled products, Non Halogenated Flame Retardant V-1 products.Supper low warpage series, HDT 110degCThis data was supplied by SABIC-IP for the Asia Pacific region. |