Flexural Modulus 5.77 GPa
837 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL ZM3242 PPE+PS (Asia Pacific)
Modified PPO* 30% mineral filled products, Non Halogenated Flame Retardant V-1 products.Supper low warpage series, HDT 110degC
Flexural Modulus 5.77 GPa
837 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Thermocomp ZM3242 PPE+PS (Asia Pacific)
Modified PPO* 30% mineral filled products, Non Halogenated Flame Retardant V-1 products.Supper low warpage series, HDT 110degCThis data was supplied by SABIC-IP for the Asia Pacific region.