Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.822 GPa | 1280 ksi | ASTM D790 |
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 8.822 GPa | 1280 ksi | ASTM D790 |
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 8.822 GPa | 1280 ksi | ASTM D790 |
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 8.822 GPa | 1280 ksi | ASTM D790 |
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 8.822 GPa | 1280 ksi | ASTM D790 |
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 8.822 GPa | 1280 ksi | ASTM D790 |
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |