A. Schulman ComAlloy® E-13819 Heat Dissipative PPS

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS); Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman ComAlloy® E-13819 Heat Dissipative PPS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Specific Gravity 1.70 g/cc
1.70 g/cc
ASTM D792
Linear Mold Shrinkage 0.0052 cm/cm

@Thickness 3.175 mm
0.0052 in/in

@Thickness 0.1250 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 63.87 MPa
9263 psi
ASTM D638
Tensile Strength, Yield 65.07 MPa
9438 psi
ASTM D638
Flexural Strength 124.35 MPa
18035 psi
ASTM D790
Flexural Modulus 8.822 GPa
1280 ksi
ASTM D790
Izod Impact, Notched 0.721 J/cm
1.35 ft-lb/in
ASTM D256
Izod Impact, Unnotched 3.68 J/cm
6.90 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 281 °C
538 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 232 °C
449 °F
ASTM D648