Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.19 GPa | 1190 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Verton NV0041EV_GY7E147 PC+ABS Preliminary data for 20% long fiber single pellet non-halogen FR color filled PC/ABSThis data was supplied by SABIC-IP for the Americas region. |