Polymer Property : Flexural Modulus = 8.10 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.07 - 8.10 GPa
300 - 1170 ksi
Average value: 5.52 GPa Grade Count:29
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% ..