Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.07 - 8.10 GPa | 300 - 1170 ksi | Average value: 5.52 GPa Grade Count:29 |
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% .. |