Polymer Property : Flexural Modulus = 7453 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 51.39 GPa
7453 ksi
Fill; EN 2562A
Ensinger TECATEC™ CF60 Polyaryletherketone (PAEK)
TECATEC™ CF60 plate is a composite of 60% woven carbon fiber laminated with a polyaryl ether ketone resin (PAEK). It is produced in a proprietary process yielding good fibre and resin integration...