Material Notes:
TECATEC™ CF60 plate is a composite of 60% woven carbon fiber laminated with a polyaryl ether ketone resin (PAEK). It is produced in a proprietary process yielding good fibre and resin integration. PAEK resins are excellent for repeated steam sterilization cycles and carbon provides metal like dimensional stability and stiffness. Carbon fibre composites are radiolucent and are ideal for external fixation devices and surgical instruments such as targeting fixtures and retractor blades. It is commonly used in medical technology (surgery, orthopaedics) and is used as targeting guides, retractor blades, fixturing assemblies, and structural components.PropertiesOutstanding strengthExcellent heat distortionGood dimensional stabilityLow moisture absorptionCorrosion resistanceExcellent chemical resistanceExcellent steam sterilization in autoclave performanceInformation Provided by Ensinger Industries, Inc.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 728.8 MPa
105700 psi
Fill; EN2597B
820.8 MPa
119000 psi
Warp; EN2597B
Tensile Modulus 54.0 GPa
7830 ksi
Warp; EN2597B
55.79 GPa
8091 ksi
Fill; EN2597B
Flexural Strength 803.79 MPa
116580 psi
Warp; EN 2562A
893.77 MPa
129630 psi
Fill; EN 2562A
Flexural Modulus 40.79 GPa
5916 ksi
Warp; EN 2562A
51.39 GPa
7453 ksi
Fill; EN 2562A
Compressive Strength 521.9 MPa
75690 psi
Fill; D 6641-01
573.9 MPa
83230 psi
Warp; D 6641-01
Compressive Modulus 52.68 GPa
7641 ksi
Warp; ASTM D6641-01
53.19 GPa
7714 ksi
Fill; ASTM D6641-01
Descriptive Properties Value Comments
Short Beam Strength 9729
psi, ASTM D2344-84, Warp