Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.4895 GPa | 71.00 ksi | ASTM D790 |
DuPont™ Surlyn® 8150 Ionomer Resin, Sodium Surlyn® 8150 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The high MAA content and .. |