Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont™ Surlyn® 8150 Ionomer Resin, Sodium

Category Polymer , Thermoplastic , Ionomer , Ionomer, Molded
Manufacturer DuPont
Trade Name Surlyn®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont™ Surlyn® 8150 Ionomer Resin, Sodium.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Surlyn® 8150 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The high MAA content and mid-range neutralization level for this grade creates an exceptional combination of strengths: toughness, low-temperature toughness, abrasion resistance, tear resistance, excellent clarity, and high stiffness compared with other grades of Surlyn®. The resin is highly suitable for injection molding, providing enhanced processability over other grades.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.970 g/cc
0.0350 lb/in³
ASTM D792
Melt Flow 4.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
condition E; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength, Ultimate 31.0 MPa
4500 psi
ASTM D638
Tensile Strength, Yield 18.6 MPa
2700 psi
50 mm/min cross speed; ASTM D638
Elongation at Break 320 %
320 %
ASTM D638
Flexural Modulus 0.4895 GPa
71.00 ksi
ASTM D790
Abrasion 301
301
NBS Index; ASTM D1630
Thermal Properties Metric English Comments
Melting Point 84.0 °C
183 °F
DSC
Vicat Softening Point 53.0 °C
127 °F
Rate B, ASTM D1525-70