Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0550 GPa | 7.98 ksi | method 1, Proc.B; ASTM D-790 |
Multibase Multi-Flex® TPE A 7318 BLK The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Flexural Modulus | 0.0550 GPa | 7.98 ksi | 1% Secant, ASTM D790 |
ExxonMobil Escorene® LD-706 High EVA Cast Coextrusion Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 15.3% vinyl acetate copolymer film resin designed for coextruded cast film applications.Applications: Coextruded meat packaging film; Sealant in c.. |
|||
Flexural Modulus | 0.0550 GPa | 7.98 ksi | ASTM D790 |
Sumitomo Chemical ESPOLEX® 3885 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |