Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Escorene® LD-706 High EVA Cast Coextrusion Film Resin  (discontinued **)

Category Polymer , Film , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene® LD-706 High EVA Cast Coextrusion Film Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Exxon Chemical.A 15.3% vinyl acetate copolymer film resin designed for coextruded cast film applications.Applications: Coextruded meat packaging film; Sealant in cast film.
Physical Properties Metric English Comments
Density 0.935 g/cc
0.0338 lb/in³
Exxon Method
Environmental Stress Crack Resistance >= 500 hour
>= 500 hour
F50, Condition A; ASTM D1693
Melt Flow 8.3 g/10 min
8.3 g/10 min
Exxon Method
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
ASTM D2240
Hardness, Shore D 29
29
ASTM D2240
Tensile Strength, Ultimate 9.60 MPa
1390 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Flexural Modulus 0.0550 GPa
7.98 ksi
1% Secant, ASTM D790
Tensile Impact Strength 324 kJ/m²
154 ft-lb/in²
23°C; ASTM D-1822
Thermal Properties Metric English Comments
Melting Point 90.0 °C
194 °F
Exxon Method
Vicat Softening Point 61.0 °C
142 °F
1000g; ASTM D-1525