Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.94 GPa | 1150 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP EFL34HL PEI (Asia Pacific) LNP LUBRICOMP* EFL34HL is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 7.94 GPa | 1150 ksi | ASTM D790 |
SABIC Innovative Plastics NORYL HM3020H PPE+PS (Asia Pacific) PPE+PS GF+MF 30% filled, FR V-1, high flow |
|||
Flexural Modulus | 7.94 GPa | 1150 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP EFL34HL PEI LNP LUBRICOMP* EFL34HL is a compound based on Polyetherimide resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractable. |