Mechanical Properties Metric English Comments
Flexural Modulus 7.551 GPa
1095 ksi
ASTM D790
Kolon KOPA® KN333G25CRBK G/F Reinforced Nylon 66
EG-resistant, high strength, dimensionally stableApplications Cooling water pipesInformation provided by API-Kolon.