Kolon KOPA® KN333G25CRBK G/F Reinforced Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Kolon
Trade Name Kopa®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kolon KOPA® KN333G25CRBK G/F Reinforced Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EG-resistant, high strength, dimensionally stableApplications Cooling water pipesInformation provided by API-Kolon.
Physical Properties Metric English Comments
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D792
Moisture Absorption at Equilibrium 0.40 %
0.40 %
60% RH; ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength 157 MPa
22800 psi
ASTM D638
Elongation at Break 8.0 %
8.0 %
ASTM D638
Flexural Strength 255 MPa
37000 psi
ASTM D790
Flexural Modulus 7.551 GPa
1095 ksi
ASTM D790
Izod Impact, Notched 0.880 J/cm
1.65 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 20.0 µm/m-°C
11.1 µin/in-°F
ASTM D696
Melting Point 255 °C
491 °F
ASTM D1525
Deflection Temperature at 0.46 MPa (66 psi) 250 °C
482 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 247 °C
477 °F
ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Constant 3.6
3.6
ASTM D150
Dielectric Strength 21.0 kV/mm
533 kV/in
ASTM D149
Arc Resistance 135 sec
135 sec
ASTM D495