Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.22 GPa | 1050 ksi | ISO 178 |
Solvay TECHNYL® C 246SI V30 PA6, 30% glass filled, DRY Description: Polyamide 6, reinforced with 30 % of glass fiber, with high impact resistance, for injection molding.Available in: Asia Pacific , Europe and North AmericaProduct Applications: Having go.. |
|||
Flexural Modulus | 7.22 GPa | 1050 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp LFZ42XXC PEEK LNP THERMOCOMP* LFZ42XXC is a compound based on Polyetheretherketone resin containing Glass Fiber, Milled Glass. Added features of this material include: Low Warpage.This data was supplied by SABIC.. |
|||
Flexural Modulus | 7.22 GPa | 1050 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP PX92248 PA 6 LNP* THERMOCOMP* PX92248 is a compound based on Nylon 6 resin containing Proprietary Filler(s). |
|||
Flexural Modulus | 7.22 GPa | 1050 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP PX92248 PA 6 LNP* THERMOCOMP* PX92248 is a compound based on Nylon 6 resin containing Proprietary Filler(s). |