Mechanical Properties Metric English Comments
Flexural Modulus 4.78 GPa
693 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Konduit MT00EL PP
LNP* Konduit* MT00EL is a Polypropylene base resin with thermal fillers. Characteristics of this grade are Thermal Conductivity and it is Low Extraactible.This data was supplied by SABIC-IP for th..
Flexural Modulus 4.78 GPa
693 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP RFI12 PA 66
LNP* LUBRICOMP* RFI12 is a compound based on Nylon 66 resin containing 10% Glass Fiber, 2% Silicone. Added feature of this material is: Wear Resistant.