Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.30 - 4.69 GPa | 188 - 680 ksi | Average value: 2.84 GPa Grade Count:66 |
Overview of materials for PVC, Extruded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Extruded". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Flexural Modulus | 4.69 - 4.69 GPa @Temperature 120 - 120 °C |
680 - 680 ksi @Temperature 248 - 248 °F |
Average value: 4.69 GPa Grade Count:1 |
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% .. |